Check Ukraine import data of d w under HS code 2713. Get import data of Ukraine for HS code 2713
Date | HS Code | Product Description | Origin Country | Quantity | Net Weight [KGS] | Total Value [USD] | Importer Name |
---|---|---|---|---|---|---|---|
30/Apr/2017 | 2713200000 | "1.Bitum Road, grade 70/100; Pour point (crystallization) determined by ASTM D 938 method equivalent to ISO 2207-80 ° C; density - 0.976 g / cm3 at 70 ° C by the method EN ISO 12185 ; penetration index (method ihly) at 25 ° C, determined by the method EN 1426 - 70; Weight - 24.190 tys.khTemperatura solidification (crystallization) determined by ASTM D 938 method equivalent to ISO 2207-80 ° C; density - 0.976 g / cm3 at 70 ° C by the method EN ISO 12185; penetration index (method ihly) at 25 ° C, determined by the method EN 1426 - 73; Weight - 25.320 thou .khTemperatura solidification (crystallization) determined by ASTM D 938 method equivalent to ISO 2207-80 ° C; density - 0.976 g / cm3 at 70 ° C by the method EN ISO 12185; penetration index (method ihly) at 25 ° C, determined by the method EN 1426 - 73; Weight - 50.180 tys.khTU bY 400091131.009-2011; STB EN 12591-2010; (EN 12591: 2009) ISO 4044-2001 on ftovyy; Weight - 99.690 tys.kh , nalyvKrayina production: BYVyrobnyk OJSC "" Mozyr Oil refinery "" " | BELARUS | ***** | 99690 | 25560.3119 | View Importer |
30/Apr/2017 | 2713200000 | "1.Bitum road mark 70/100 TU BY 400091131.009-2011; STB EN 12591-2010 (EN 12591: 2009) meets the requirements of ISO 4044-2001Temperatura softening the ring and ball 50.8 ° C; penetration index - 0.1, temperature brittleness in fraasu - -21 ° C, resistance to zatvedeninnya at 163hrad.S: -zalyshkova penetration 69% -increasing the softening temperature of 5.1 ° C; -change mass (absolute value) 0.06% dynamic viscosity at 60 ° c - 283 Pa.s, kinematic viscosity at 135 ° c - 380 mm2 / s; flash point - 297 ° c; solubility - 99.95% temperature crystallization (ASTM D 938) - 80 ° C, with temperature density 70hrad.S round (EN ISO 12185) - 0.976 g / cm3; penetration index (penetration) at 25 ° C method (needles) (EN 1426) - 70.Vaha - 49010 kh.Vyrobnyk OAO "" Mozy'rskij neftepererabatыvayuschyy plant " "Country of origin - BY.Torhivelna mark - Mozy'rskij neftepererabatыvayuschyy zavodVykorystovuetsya for construction and repair of roads." | BELARUS | ***** | 49010 | 12643.6395 | View Importer |
29/Apr/2017 | 2713200000 | "1.Bitum road mark 70/100 TU BY 400091131.009-2011 STB EN 12591-2010 (EN 12591: 2009) complies with ISO 4044-2001.Temperatura softening the ring and ball 47.6; 48.4hrad.S; Index penetration of -0.3, -0.4. Fraasu temperature brittleness in -21hrad.S, resistance to zatverdeninnya at 163hrad.S: -zalyshkova 69% penetration - increasing the softening temperature 5.1hrad.S; -change mass (absolute value) 0 06% dynamic viscosity at 60 ° c 283Pa.s, kinematic viscosity at 135 ° c 380 mm2 / s; flash point 297 ° c; solubility of 99.95%, crystallization temperature (ASTM D 938) - 80hrad.Tselsiya, with density emperaturi 70 hrad.Tselsiya (EN ISO 12185) - 0,976h / cm3; penetration index (penetration) at 25 hrad.Tselsiya method (needles) (EN 1426) - 91; 84.Vaha - 147580kh.Vyrobnyk: OAO "" Mozy'rskij neftepererabatыvayuschyy plant "," Country of origin - BY.Torhivelna mark - Mozy'rskij neftepererabatыvayuschyy plant. " | BELARUS | ***** | 147580 | 41466.85193 | View Importer |
29/Apr/2017 | 2713200000 | "1.Bitum road mark 70/100 TU BY 400091131.009-2011 STB EN 12591-2010 (EN 12591: 2009) complies with ISO 4044-2001.Temperatura softening the ring and ball 49.2hrad.S; penetration index 0.0 kryhkostipo Fraasu -20hrad.S temperature, resistance to zatverdeninnya at 163hrad.S: -zalyshkova 68% penetration - increasing the softening temperature 5.0hrad.S; -change mass (absolute value) 0.03% dynamic viscosity at 60 ° c 298Pa.s, kinematic viscosity at 135 ° c 472 mm2 / s; flash point 301 ° c; solubility of 99.95%, crystallization temperature (ASTM D 938) - 80hrad.Tselsiya; density with temperature Uri hrad.Tselsiya 70 (EN ISO 12185) - 0,976h / cm3; penetration index (penetration) at 25 hrad.Tselsiya method (needles) (EN 1426) -89.Vaha - 48420kh.Vyrobnyk: OAO "" Mozy'rskij neftepererabatыvayuschyyzavod " "Country of origin - BY.Torhivelna mark - Mozыrskyyneftepererabatыvayuschyy plant." | BELARUS | ***** | 48420 | 12475.83701 | View Importer |
29/Apr/2017 | 2713200000 | "1.Bitum road mark 70/100 TU BY 400091131.009-2011 STB EN 12591-2010 (EN 12591: 2009) complies with ISO 4044-2001.Temperatura softening the ring and ball 48.4hrad.S; penetration index - 0.4 brittleness temperature by Fraasu -21hrad.S, resistance to zatverdeninnya at 163hrad.S: -zalyshkova 69% penetration - increasing the softening temperature 5.1hrad.S; -change mass (absolute value) 0.06%, a dynamic ' viscosity at 60 ° c 283Pa.s, kinematic viscosity at 135 ° c 380 mm2 / s; flash point 297 ° c; solubility of 99.95%, crystallization temperature (ASTM D 938) - 80hrad.Tselsiya, density at temp aturi 70 hrad.Tselsiya (EN ISO 12185) - 0,976h / cm3; penetration index (penetration) at 25 hrad.Tselsiya method (needles) (EN 1426) - 84.Vaha - 48200kh.Vyrobnyk: OAO "" Mozy'rskij neftepererabatыvayuschyy plant "" Country of origin - BY.Torhivelna mark - Mozy'rskij neftepererabatыvayuschyy plant. " | BELARUS | ***** | 48200 | 13545.15514 | View Importer |
29/Apr/2017 | 2713200000 | "1.Bitum road mark 70/100 TU BY 400091131.009-2011; STB EN 12591-2010 (EN 12591: 2009) meets the requirements of ISO 4044-2001Temperatura softening the ring and ball 47.6, 47.0 degrees. C penetration index - 0.3, temperature brittleness in fraasu - -21 ° C, resistance to zatvedeninnya at 163hrad.S: -zalyshkova penetration 69% -increasing the softening temperature of 5.1 ° C; -change weight (absolute value) 0.06% dynamic viscosity at 60 ° c - 283 Pa.s, kinematic viscosity at 135 ° c - 380 mm2 / s; flash point - 297 ° c; solubility - 99 95% crystallization temperature (ASTM D 938) - 80 ° C, at a density rate eraturi 70hrad.S (EN ISO 12185) - 0.976 g / cm3; penetration index (penetration) at 25 ° C method (needles) (EN 1426) - 92; 93.Vaha - 164,450 kh.Vyrobnyk OAO "" Mozy'rskij neftepererabatыvayuschyy plant "," Country of origin - BY.Torhivelna mark - Mozy'rskij neftepererabatыvayuschyy zavodVykorystovuetsya for construction and repair of roads. " | BELARUS | ***** | 164450 | 42335.54488 | View Importer |
29/Apr/2017 | 2713200000 | "1.Bitum road mark 70/100 TU BY 400091131.009-2011 STB EN 12591-2010 (EN 12591: 2009) complies with ISO 4044-2001.Temperatura softening the ring and ball 49.0 ° C; penetration index - 0.3, -0.1 kryhkostipo temperature -20 ° C Fraasu; zatverdeninnya resistance at 163 ° C, -zalyshkova 68% penetration - increasing the softening temperature 5.0hrad.S; -change mass (absolute value) 0 03% dynamic viscosity at 60 ° c 298Pa.s, kinematic viscosity at 135 ° c 472 mm2 / s; flash point 301 ° c; solubility of 99.95%, crystallization temperature (ASTM D 938) - 80hrad.Tselsiya; density with topics temperature to 70 hrad.Tselsiya (EN ISO 12185) - 0,976h / cm3; penetration index (penetration) at 25 hrad.Tselsiya method (needles) (EN 1426) -82, -123 480 85.Vaha kh.Vyrobnyk: OAO "" Mozy'rskij neftepererabatыvayuschyyzavod "" Country of origin - BY.Torhivelna mark - Mozыrskyyneftepererabatыvayuschyy plant. " | BELARUS | ***** | 123480 | 31810.70128 | View Importer |
29/Apr/2017 | 2713200000 | "1.Bitum Road, grade 70/100; Pour point (crystallization) determined by ASTM D 938 method equivalent to ISO 2207-80 ° C; density - 0.976 g / cm3 at 70 ° C by the method EN ISO 12185 ; penetration index (method ihly) at 25 ° C, determined by the method EN 1426 - 93; THAT bY 400091131.009-2011; STB EN 12591-2010, (EN 12591: 2009) ISO 4044-2001, oil; Weight - 24.890 tys.kh, nalyvKrayina production: BYVyrobnyk OJSC "" Mozyr Oil refinery "." " | BELARUS | ***** | 24890 | 6381.744155 | View Importer |
29/Apr/2017 | 2713200000 | "1.Bitum road mark 70/100 TU BY 400091131.009-2011 STB EN 12591-2010 (EN 12591: 2009) complies with ISO 4044-2001.Temperatura softening the ring and ball 47.8hrad.S; penetration index - 0.3, the temperature in Fraasu -21hrad.S brittleness, resistance to zatverdeninnya at 163hrad.S: -zalyshkova 69% penetration - increasing the softening temperature 5.1hrad.S; -change mass (absolute value) 0.06% dynamically 'viscosity at 60 ° c 283Pa.s, kinematic viscosity at 135 ° c 380 mm2 / s; flash point 297 ° c; solubility of 99.95%, crystallization temperature (ASTM D 938) - 80hrad.Tselsiya; density at temperature aturi 70 hrad.Tselsiya (EN ISO 12185) - 0,976h / cm3; penetration index (penetration) at 25 hrad.Tselsiya method (needles) (EN 1426) - 91.Vaha - 71150kh.Vyrobnyk: OAO "" Mozy'rskij neftepererabatыvayuschyyzavod " "Country of origin - BY.Torhivelna mark - Mozыrskyyneftepererabatыvayuschyy plant." | BELARUS | ***** | 71150 | 19996.94066 | View Importer |
29/Apr/2017 | 2713200000 | "1.Bitum road mark 70/100 TU BY 400091131.009-2011 STB EN 12591-2010 (EN 12591: 2009) complies with ISO 4044-2001.Temperatura softening the ring and ball 47.6; 48.4hrad.S; Index penetration -0.3; -0.2; kryhkostipo Fraasu -21hrad.S temperature, resistance to zatverdeninnya at 163hrad.S: -zalyshkova 69% penetration - increasing the softening temperature 5.1hrad.S; -change mass (absolute value) 0.06 % dynamic viscosity at 60 ° c Pa.s 283; kinematic viscosity at 135 ° c 380 mm2 / s; flash point 297 ° c; solubility of 99.95%, crystallization temperature (ASTM D 938) - 80hrad.S; density with temperature round 70 ° C (EN ISO 12185) - 0,976h / cm3; penetration index (penetration) at 25 hrad.Tselsiya method (needles) (EN 1426) - 93; 91; 90.Vaha - 73310kh.Vyrobnyk: OAO " "Mozy'rskij neftepererabatыvayuschyy plant", "Country of origin - BY.Torhivelna mark - Mozy'rskij neftepererabatыvayuschyy plant." | BELARUS | ***** | 73310 | 21150.26172 | View Importer |
29/Apr/2017 | 2713200000 | "1.Bitum road mark 70/100 TU BY 400091131.009-2011; STB EN 12591-2010 (EN 12591: 2009) meets the requirements of ISO 4044-2001Temperatura softening the ring and ball 48.4 ° C; penetration index - -0.4; temperature brittleness in fraasu - -21 ° C, resistance to zatvedeninnya at 163hrad.S: -zalyshkova penetration 69% -increasing the softening temperature of 5.1 ° C; -change mass (absolute value) 0.06% dynamic viscosity at 60 ° c - 283 Pa.s, kinematic viscosity at 135 ° c - 380 mm2 / s; flash point - 297 ° c; solubility - 99.95% temperature crystallization (ASTM D 938) - 80 ° C, with temperature density 70hrad.S round (EN ISO 12185) - 0.976 g / cm3; penetration index (penetration) at 25 ° C method (needles) (EN 1426) - 84.Vaha - 48,510 kh.Vyrobnyk OAO "" Mozy'rskij neftepererabatыvayuschyy plant " "Country of origin - BY.Torhivelna mark - Mozy'rskij neftepererabatыvayuschyy zavodVykorystovuetsya for construction and repair of roads." | BELARUS | ***** | 48510 | 12514.64355 | View Importer |
29/Apr/2017 | 2713200000 | "1 mark 70/100 bitumen - weight of goods 247,040 kh.TU BY 400091131.009-2011 STB EN 12591-2010 (EN 12591: 2009) complies with ISO 4044-2001.Penetratsiya at 25 deg. C - 84; 86 (0.1 mm) .Temperatura rozmyahchennya the ring and layer - 47.6; 48.4 ° C.;. Index penetration - (- 0.4). hrupkosti on Fraasu temperature: (- 21 ° C) Resistance to hardening at 163 deg. C.: - 69% of the final penetration .- rozmyahshennya increase in temperature of 5.1 deg. C, the change in mass (absolute value) of not more than 0.06% .Dynamichna viscosity at 60 deg. C 283 .- Pas s.Kinematychna viscosity at 135 deg. C - 380 mm2 / s.Temperatura flash 297 deg. S.Rozch ment crystallization .Temperatura 99.95% (ASTM D 938) - 80 deg. S.Hustyna at 70 deg. C (EN ISO 12185) - 0.976 g / sm3.Indeks penetration (penetration) at 25 ° C (method ihly) (EN 1426) - 84,86.Vyrobnyk: OAO "" Mozy'rskij neftepererabatыvayuschyy plant "," Country of origin - BYTorhivelna mark - "" Mozy'rskij neftepererabatыvayuschyy plant "." " | BELARUS | ***** | 247040 | 68846.31737 | View Importer |
29/Apr/2017 | 2713200000 | "1.Bitum road mark 70/100 TU BY 400091131.009-2011 STB EN 12591-2010 (EN 12591: 2009) complies with ISO 4044-2001.Temperatura softening the ring and ball 48.4hrad.S; penetration index - 0.4temperatura kryhkostipo Fraasu -21hrad.S, resistance to zatverdeninnya at 163hrad.S: -zalyshkova penetration 69% -increasing softening temperature 5.1hrad.S; -change mass (absolute value) of 0.06, the dynamic viscosity at 60 283Pa.s ° c, kinematic viscosity at 135 ° c 380mm2 / s 297hrad.S flash point, solubility of 99.95%, crystallization temperature (ASTM D 938) - 80hrad.Tselsiya; density at o and 70 hrad.Tselsiya (EN ISO 12185) - 0,976h / cm3; penetration index (penetration) at 25hrad.Tselsiya method (needles) (EN1426) - 84.Vaha: 24040khVyrobnyk: OAO "" Mozy'rskij neftepererabatыvayuschyyzavod "" Country of origin - BY.Torhivelna mark - Mozыrskyyneftepererabatыvayuschyy plant. " | BELARUS | ***** | 24040 | 6827.693761 | View Importer |
29/Apr/2017 | 2713200000 | "1 mark 70/100 bitumen - weight of goods 169,140 kh.TU BY 400091131.009-2011 STB EN 12591-2010 (EN 12591: 2009) complies with ISO 4044-2001.Penetratsiya at 25 deg. C - 80; 82; 92; 93 (0.1 mm) .Temperatura rozmyahchennya the ring and layer - 47.0, 47.6, 49.2, 49.8 ° C.;. Index penetration - (0,0 - 0 3). hrupkosti on Fraasu temperature: (- 20, -21 ° C) Resistance to hardening at 163 deg. C.: - 69% of the final penetration .- rozmyahshennya increase in temperature of 5.1 deg. C, the change in mass ( absolute value) of not more than 0.06% .Dynamichna viscosity at 60 degrees. S.- 283 Pa s.Kinematychna viscosity at 135 deg. C - 380 mm2 / s.Temperatura outbreak 2 97 degrees. S.Rozchynennya 99.95% .Temperatura crystallization (ASTM D 938) - 80 deg. S.Hustyna at 70 deg. C (EN ISO 12185) - 0.976 g / sm3.Indeks penetration (penetration) at 25 ° C (method ihly) (EN 1426) - 80,82,92,93.Vyrobnyk: OAO "" Mozy'rskij neftepererabatыvayuschyy plant "," Country of origin - BYTorhivelna mark - "" Mozy'rskij neftepererab atыvayuschyy plant "" " | BELARUS | ***** | 169140 | 47140.23033 | View Importer |
28/Apr/2017 | 2713200000 | "1.Bitum road mark 70/100 TU BY 400091131.009-2011 STB EN 12591-2010 (EN 12591: 2009) complies with ISO 4044-2001.Hlybyna ponyknennya needles (penetration) in 25hrad.S - 77, the temperature posted ' conditioner is required on the ring and ball 49.0hrad.S, resistance to zatverdeninnya at 163hrad.S: -zalyshkova 68% penetration - increasing the softening temperature of 4.8% - the change in mass (absolute value) 0.03% flash 308hrad .S; solubility 99.95% penetration index of -0.4, the dynamic viscosity at 60hrad.S 195Pa.s the temperature brittleness in Fraasu -17hrad.S, kinematic viscosity at 135hrad.S 447mm2 / s.Temperatura krystaliz ted 79hrad.S (ASTM D938-12); density at 70hrad.S (STB ISO 12185-2007 (ISO 12185: 1996, IDT) 0,968h / cm3; penetration index (penetration) at 25hrad.S (STB EN 1426 -2009 (EN1426-2009, IDT) 77.. " | BELARUS | ***** | 115900 | 30498.21417 | View Importer |
Our market research report and Ukraine export statistics of d w covers market share of Ukrainian companies and market price of sunglass. This helps you to do market analysis on the basis of price, company, etc. perfectly and study market size of sunglass in Ukraine. Few shipment records with a small number of important columns from Ukraine export data of sunglass are given above. Other hidden fields such as Ukrainian Exporter Name with Address, Foreign er Name with Address, Value, Quantity, Origin & Destination Country and more are also covered in Ukraine customs data of sunglass. To view more shipment records of sunglass export data of Ukraine, you can set a filter by Country Name or HS Code on the left side.
To get complete sunglass export statistics of Ukraine, simply fill the Request Demo Form. You can also drop your queries through info@exportgenius.in or +91-11-47048012.
Are you looking for Ukraine buyers or importers of d w